FERRIT EFD KJARNI

FERRIT EFD KJARNI

product-705-272

 

MYNDAN

G.W

STÆRÐ(mm)

A

B

C

D

C

F

G

H

EFD20

9

20.0±0.6

15.4±0.5

8.9±0.2

6.7±0.2

7.7±0.3

10.0±0.3

0.2±0.1

3.6±0.2

EFD21A

9

20.8±0.6

15,4 mín

8.9±0.2

6.7±0.2

7.7±0.3

10.0±0.3

0.2±0.1

3.6±0.2

EFD21B

9.7

21.0±0.5

15,4 mín

8.9±0.2

6.7±0.2

8.0±0.3

10.3±0.3

\

3.6±0.2

EFD25,6

19

25.6±0.7

19.5±0.7

11.4±0.3

9.1±0.3

9.3±0.3

12.5±0.3

0.6±0.1

5.2±0.3

EFD31

25

30.8±0.8

23,2 mín

14.4±0.3

8.8±0.2

11.2±0.3

15.0±0.3

0.3±0.2

4.8±0.2

EFD34

29.6

34.0±0.6

24.0±0.5

17.0±0.3

5.0±0.2

18.0±0.3

23.0±0.3

\

3.0±0.2

EFD40/45/11

60

40.5±0.7

30.0mín

16.6±0.3

10.6±0.2

16.3±0.3

22.5±0.3

\

6.6±0.2

EFD40/44/8

44

40.0±0.7

29,5 mín

19.9±0.4

8.0±0.2

17.1±0.3

22.0±0.3

\

4.0±0.2

EFD43/53/4.4

63.6

43.0±0.8

28,5 mín

21.6±0.4

7.6±0.25

19.3±0.3

26.5±0.3

\

4.4±0.25

EFD43/44/3.2

49.2

43.4±0.8

33,5 mín

22.3±0.4

8.0±0.25

17.1±0.3

22.2±0.3

\

3.2±0.25

EFD45/50

67

45.2±0.8

33.3±0.8

24.0±0.4

7.8±0.2

18.0±0.3

24.7±0.3

\

4.0±0.2

EFD52,5

118

52.5±1.1

39 mín

22.5±0.4

13.0±0.3

19.9±0.3

27.0±0.3

\

7.5±0.3

 

MYNDAN

FRÆÐI

AL±25%(nH/N^2)

N.W(g)

C1mm-1

Lemm

Aemm2

Vemm3

ZP40

EFD20

1.52

47.0

31.0

1460.0

1150

7.9

EFD21A

1.57

49.3

31.0

1460.0

1400

7.9

EFD21B

1.57

49.3

31.4

1540.0

1450

8.6

EFD25,6

1.00

57.0

58.0

3300.0

2000

16.5

EFD31

0.99

68.2

69.1

4712.0

2000

23.0

EFD34

1.90

95.0

50.0

4750.0

1400

33.5

EFD40/45/11

1.02

108.8

106.5

10951.0

2300

55.0

EFD40/44/8

1.35

102.8

75.5

7750.0

1700

38.0

EFD43/53/4.4

1.14

111.3

99.8

11113.0

2000

59.0

EFD43/44/3.2

1.41

102.0

72.1

7352.0

1500

43.0

EFD45/49

1.08

108.0

97.7

10356.2

2700

60.0

EFD52,5

0.78

132.0

168.0

23250.0

2750

109.0